PETG stringing
PETG Stringing: A Controlled Checklist
Hairs between parts are a symptom, not a retraction preset. Dry the grade you actually loaded, then change one setting from that machine's own profile.
Updated November 2026 · Diagnostic, not a product ranking
Lena OrtizWriter
Log one comparison print before you edit
Stringing is a hair left while the nozzle travels. Oozing is a blob or a drip when the nozzle should not be extruding. Bambu treats bubbles, holes, and a rough surface as wet filament, which is a different branch from a retraction edit.
Print two small posts with a gap, or the test that maker already ships. Save the file. Write the printer, direct drive or Bowden, nozzle diameter, brand and grade, profile name, nozzle temperature, retraction length, and retraction speed. Change nothing on this first print. The photo is the baseline.
- Name the symptom: hairs, blobs, bubbles, or a rough surface.
- Name the machine path: Prusa direct drive, Prusa MINI Bowden, or Bambu direct drive. Do not guess.
- Copy the loaded profile. Do not type a temperature from memory.
- Reprint only after one change. If the hairs do not change, revert that change before the next one.
Moisture is the first change, and only if the grade is known
Prusa's stringing article says to try a different spool, because moisture causes a lot of stringing. Bambu's PETG guide says obvious stringing means the filament is damp and needs drying, and their stringing page puts damp filament first, then a sealed box with desiccant.
Dry only with a row on the drying guide that names your grade and your equipment. Expected result on the reprint: fewer bubbles and fewer hairs, with the same profile. If the surface was already smooth and the hairs do not change, revert the idea that moisture was the cause and go to the profile step. Do not dry this spool in a kitchen oven. Do not enclose an A1, and do not bed-dry on an A1, A1 mini, P1P, or A2L.
If you cannot dry a Bambu PETG HF spool yet, Bambu's usage guide gives one fallback: Generic PETG HF parameters, nozzle 220 C and volumetric speed 16 mm3/s, instead of the default Bambu PETG HF profile. That fallback is for wet PETG HF in Bambu Studio. It is not a Prusament temperature and it is not a retraction length. Print quality will still move as the spool dries. The expected result is a more stable wet print, not a finished calibration.
Load the factory profile before you invent a number
Prusa says to start from the official preset, and that stringing comes from a high temperature or the wrong retraction. Their PETG article says stringing can be moderated with higher retraction and a lower nozzle temperature, and then tells you to use the PrusaSlicer profiles. Cooling helps detail and stringing. Fan off makes a tougher part. Their practical note is fan off for the first layers, then about half power. That fan change is its own step, later, not a companion to a temperature edit.
The PETG article's temperatures are 230 C then 240 C at the nozzle, and 85 C then 90 C on the bed. A comment on that page says PrusaSlicer 2.9.4 uses 250 C and 85 C on the bed for Prusament PETG. No staff reply in the opened comments confirms which number is current. Write down the number the slicer actually loaded. The profile is the baseline. The article is not a second baseline you apply on the same print.
Bambu's material table lists a nozzle range, not one setpoint: PETG 240 to 270 C, PETG HF 230 to 260 C, PETG Translucent 230 to 260 C, each plus or minus 10 C. Their stringing page says to lower the nozzle temperature if it is too high, without a universal drop. Expected result after switching from a custom profile back to the factory profile: fewer hairs, walls still solid. If you were already on that profile, this step changes nothing, and you record that.
Then change one setting, and say what should happen
Pick the first row that matches the baseline. Do the one change. Reprint the same two posts. If the expected result does not show up, revert before the next row.
One change per reprint. Revert when the expected result does not appear. Lengths are not interchangeable.
Swipe sideways. The first column stays visible.
| You are on | One change | Expected result | Stop if |
|---|---|---|---|
| Any PETG, after the factory profile is loaded, and moisture is handled or ruled out. | Lower the nozzle temperature by 5 to 10 C from the temperature you just printed. That drop is Prusa's stringing article. Bambu says only to lower it appropriately. | Fewer hairs. Layers still hold together when you flex a thin wall. | Layers split or the surface turns matte and weak. Revert. Do not also change retraction on this reprint. |
| Prusa MK2.5/S or MK3/S/+, direct drive, still stringing after the temperature reprint. | Set retraction length no higher than the 2 mm maximum in Prusa's article. Change length or speed, not both. Leave wipe and retract on layer change as the preset has them. | Shorter hairs between the posts. Lines on the part stay continuous. | Gaps, clicking, or a clog. Revert. Do not copy the MINI's 3.2 mm onto this machine. |
| Prusa MINI or MINI+, Bowden. | Start from the preset default of 3.2 mm. Do not replace it with the 2 mm MK3 maximum. Prusa says avoid crossing perimeters helps this Bowden machine in particular. | Fewer hairs across the gap, without under-extrusion at the start of a line. | You imported an MK3 or a Bambu length. Put the MINI preset back. |
| Bambu printer, direct drive, still stringing after drying and the factory profile. | Increase retraction length or speed a little, and keep length no greater than 2 mm. Bambu also says to move parts closer and enable Avoid crossing wall. | Fewer hairs. No new clog and no missing line at the start of a perimeter. | A clog, or gaps. Their stringing page says a retraction length that is too large can clog. Revert. The 2 mm figure is a ceiling, not a target you must hit. |
| MK4, MK4S, XL, CORE One, or any machine not named above. | Do not import a retraction length from a different Prusa or from Bambu. Stay on that printer's factory profile. One travel change is allowed: fewer gaps between parts. | The factory profile either fixes the hairs or it does not. You will know which. | You need a length these pages did not publish. That number is unknown here. Ask that maker before you type one in. |
Travel and cooling, still one at a time
Prusa lists travel tools that are already in the presets: wipe while retracting, retract on layer change, and only retract when crossing perimeters so any ooze stays inside the part. Minimum travel after retraction defaults to 1 mm. Raising it shortens the print and increases stringing, so it is the wrong direction if hairs are the problem. Sequential printing can stop strings between objects. PrusaSlicer warns if the toolhead might hit a finished part. Watch that print.
Bambu's stringing page says long travel with too little retraction lets melt drip, and that a cluttered plate makes it worse. Move models closer. Enable Avoid crossing wall. A worn nozzle or the wrong nozzle size in the slicer is a later hardware check, not this step.
Fan is a separate reprint. On a Prusa PETG profile, the article's sequence is fan off for the first layers, then about half. Expected result: less stringing and less deformation. If you wanted maximum toughness, they say try the fan off, and you accept the stringing trade. Do not change fan and temperature together.
On an enclosed Bambu printer, PETG can soften in the extruder if the chamber is hot. The material table says to open the door or remove the top glass when the bed is above 60 C in the prose, and the plate table says the cover removal is recommended if the bed is above 70 C. Those two sentences disagree. Do not enclose an A1 to create the opposite problem. A1 stringing is not a chamber problem you solve with a box.
Hardware, then the maker, not a hotter nozzle
Prusa says a long run of one material, such as PETG, can leave a film in the nozzle that hairs stick to. Clean that residue before the next diagnostic print. If you recently rebuilt the hotend, check the assembly, including thermal paste on the heatbreak threads. Expected result: the comparison print changes after the cleaning alone. If it does not, the film was not the cause.
Bambu says a nozzle diameter that does not match the sliced profile, or a worn nozzle, pushes out too much melt. Confirm the sliced nozzle is the nozzle in the toolhead. Replace a worn nozzle only after that check. PETG-CF needs a hardened nozzle on their compatibility table. Plain PETG does not. Do not buy a hardened nozzle because a PETG spool strung.
Escalate when one documented change at a time has not moved the comparison, or a blob from oozing stalls an axis. Prusa's comments on the PETG article point that layer-shift case to Prusa support with photos. Bambu's stringing page asks for a ticket with logs and photos. Bring the log from the first section.
The heat gun in Prusa's article is about 200 C, aimed at hairs for one or two seconds, and they warn that longer contact can deform the part. A lighter is mentioned only with the same warning. That is a cleanup of hairs already printed. It is not step one, and it is not a Bambu procedure on the pages opened here.
Sources opened for this page
Each limit above is tied to the page that states it. This site did not print a stringing test. Primary pages: Prusa, Stringing and oozing, Prusa, PETG, Bambu, Stringing and oozing, Bambu, PETG Usage Guide, Bambu, filament material table, and Bambu, A1 FAQ.
- Prusa, Stringing and oozing: causes, the 2 mm maximum on MK2.5/S and MK3/S/+, the MINI Bowden default of 3.2 mm, the 5 to 10 C nozzle drop, preset travel options, moisture, nozzle film, and the heat-gun cleanup.
- Prusa, PETG: 230 C / 240 C nozzle, 85 C / 90 C bed, fan guidance, stringing as a listed weakness, and the instruction to use PrusaSlicer profiles. A reader comment claims the 2.9.4 preset differs. That comment is not treated as the preset.
- Bambu, Stringing and oozing: damp filament first, travel, retraction ceiling of 2 mm, avoid crossing walls, temperature, and worn or mismatched nozzles.
- Bambu, PETG Usage Guide: moisture photos, the wet PETG HF fallback at 220 C and 16 mm3/s, and the grouped drying row.
- Bambu, Filament guide material table: nozzle ranges and the chamber-cover notes that disagree with each other at 60 C and 70 C.
- Bambu, A1 FAQ: do not enclose the A1. Open-frame printers are a poor default for large ABS and ASA parts, which is a different problem from PETG hairs.
- The drying guide on this site holds the grade temperatures. They are not repeated as if they were stringing settings.
Conflicts and unknowns
Left open on purpose.
- Prusa PETG article temperatures versus the reader-reported PrusaSlicer 2.9.4 preset. The live preset file was not opened. Use the number on your screen as the baseline, and record it.
- Retraction length for MK4, MK4S, XL, and CORE One. Not stated on the stringing article. Unknown here.
- Bambu's 2 mm retraction ceiling versus Prusa's 3.2 mm MINI default. Both are manufacturer-documented. Neither transfers.
- Bambu chamber relief for PETG: prose says when the bed is above 60 C, the plate table says above 70 C.
- A single PETG drying temperature. See the drying guide. Do not pick one so the stringing test looks tidy.
Who should skip this page
Skip a universal retraction length
Prusa's stringing article sets a 2 mm maximum on the MK2.5/S and MK3/S/+, and a 3.2 mm default on the Bowden MINI/MINI+. Bambu says to keep retraction no greater than 2 mm. Those are different machines. MK4, XL, and CORE One retraction lengths were not stated on the pages opened here.
Skip enclosing an A1 to stop strings
Bambu's A1 FAQ says they do not recommend enclosing the A1. An enclosure is not a stringing fix on that printer.
Skip the heat gun as the first step
Prusa describes a heat gun at about 200 C for one or two seconds only as a way to melt hairs that are already on the part. Longer than that can deform the part. It does not find the cause.
Who it's not for
A slicer profile to download, or a shopper's list of dryers and nozzles. Drying temperatures live on the drying guide. A new nozzle comes after the comparison print shows wear or a size mismatch.
Frequently asked questions
- Should I raise retraction on every PETG printer?
- No. Bambu's stringing page puts drying first. Then use the factory profile for that printer. Prusa's MINI Bowden preset defaults to 3.2 mm. Their MK2.5/S and MK3/S/+ maximum is 2 mm. Bambu says not to set retraction length above 2 mm, because a longer pull can clog. Do not paste one of those numbers onto a different machine.
- What nozzle temperature should PETG use?
- Start from the profile that slicer loaded for that grade and write the number down. Prusa's PETG article says 230 C on the first layer and 240 C after, with the bed at 85 C then 90 C. A reader comment on that article says PrusaSlicer 2.9.4 shows 250 C. Prusa staff do not confirm the preset in the comments that were opened. Bambu's material table lists PETG at 240 to 270 C, PETG HF and Translucent at 230 to 260 C, each plus or minus 10 C. The only 220 C figure opened here is Bambu's Generic PETG HF fallback when the spool is still wet.
- Does stringing mean the filament is wet?
- It can. Bambu shows obvious stringing, bubbles, holes, and a rough surface as moisture in PETG. Prusa says a wet spool can string and tells you to try a different spool. If the comparison print is bubbly, dry that grade and reprint before you touch retraction. If the hairs stay and the surface is already smooth, moisture is the weaker hypothesis.
Related 3D printer guides
How to Dry Filament (PETG, TPU, PLA)
Match the grade to the dryer and the spool. Where Prusa and Bambu disagree, both figures stay on the page. A kitchen oven is not the default.
3D Print Not Sticking to the Bed
Name the plate before you wash it. Prusa and Bambu do not share a cleaner, and PETG on smooth PEI can be stuck too well, not too little.
PLA vs PETG: Which Should You Print?
Stringing, a wet spool, or a loose first layer is a fix on the printer you already have. A different printer comes after those checks, and only for the job that printer can actually do.
3D printer setup tips: what to do before your first print
What to do before a first print on any printer: where it sits, how to calibrate, when to wash the plate, and how much setup each scored machine still needs.